Friday, July 22, 2011

RE: [MW:11855] Maximum Allowable Offset In Welded Joints // ASME SEC VIII div2 //

Hi all,

 

It is maximum only,

 

Ie. Maximum allowable offset is 10mm, more than 10 mm means it is not acceptable.

 

Thanks and Regards................?

cid:image001.jpg@01CC3048.5836D9B0

Lakshman Kumar.B|Manager- QA/QC |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

Please note that my "Lanco group" mail is not working properly at some times, request you keep a copy to personal mail ID lakshmankumar4@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of VIshal Sapkale
Sent: Thursday, July 21, 2011 3:57 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11847] Maximum Allowable Offset In Welded Joints // ASME SEC VIII div2 //

 

Dear,

 

It should be max only. if it is min, its mean max value will be anything

Regards

Vishal

 

On Mon, Jul 18, 2011 at 10:48 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:

please refer the attchement, seems to be a typo error while revising code in 2007, they may correct it in the next edition

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Dear,






Regards,
Vishal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...