Re: [MW:11819] UT TESTING MIN. AND MAXIMUM THICKNESS FOR PIPE .

there is no definite limit on the thickness of materials, depending on
the type of materials and UT technique you use.

you can refer to several online resources on one of them:
http://ndt-specialist.com

Regards
Achmed

2011/7/18, s karthik <karthi.krish41@gmail.com>:
> Hi All,
>
> If you inspect long seam weld means we have to select the probe
> angle ID/OD=sin(Optimal inspection Angle).
> Normally we have do the Ultrasonic Friction Weld in 5mm stem.
> Regards,
> karthik,
> Coimbatore.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...