[MW:11820] Re: Using 10018-G Electrode replacing 9018-G in WB-36 Material with out qualifying PQR.

Dear Kannayeram,

Is this mentioned in code any where???


Regards,

Jose

On Jul 16, 8:18 pm, kannayeram gnanapandithan <kgpandit...@gmail.com>
wrote:
> No, since it is G classification, u have to qualify, do not overmatch
>
>
>
>
>
>
>
> On Tue, Jul 12, 2011 at 1:05 PM, JOSE SEBASTIAN <josese...@gmail.com> wrote:
> > Dear Friends,
>
> > We have a qualified PQR for WB-36 Material using E 9018-G material and
> > we are using it in site.Now a vendor is supplying us 10018-G which is
> > more available.
>
> > Can I use 10018-G instead of 9018-G without qualifying PQR.I think in
> > both cases essential varialbles are same....
>
> > Also Is there any problem in using 9018-G instead of 10018-G without
> > qualifying PQR....
>
> > Regards,
> > Jose
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...