Dear Sandy,

i think there will not be any effect on both metallurgical or mechanical properties and if u want to ensure of that u can conduct DPT examination on exposed surface,, i have did that b4.

On Thu, Jul 14, 2011 at 7:22 AM, sandy <sandeepdhiman63@gmail.com> wrote:
Dear All
what can be the effect of machining on properties of steel to reduce
thickness of non alloy steel plates due to non-availability of
required thickness?
does machining with coolant help in any way?
effect on mechanical properties, metallurgical properties etc.
Please give your valuable suggestion.

Regards
Sandeep Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Best regards,
 
Tarek Yehia
QA/QC Inspection Engineer
BEMCO Steel Industries, Jeddah, Saudi Arabia
E-mail: t.yehia2009@gmail.com
            
Cell. #+966546154198
          +966567726160

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...