Thursday, July 14, 2011

Re: [MW:11729] Clarification of PQR/WPS in FCAW process

Dear arvinda,

the thickness & welding position  both are essential variables.In wps what mention for the E71-T-1 Wheather it is single shield or 80-20 .
generally E71-T-1c with 100% co2 ,E 71-T-1M is 80%ar+20%co2 .You can refere from the gas characteristics in wps .
3G(UP) WILL QUALIFY YOUR PROCEDURE 1G -2G -3G (UP) ONLY.

REFERENCE : AWS D 1.1

REGARDS

DINESH

On Wed, Jul 13, 2011 at 4:42 PM, arvinda shan <arvindashan@gmail.com> wrote:
Dear Experts,
 
I need some clarification in document review. PQR qualified in FCAW process for 27 mm plate in 3G position. WPS is prepared for structural joint for 34 mm in all positions.What is the essential one?
 
  1. In FCAW proces PQR , Electrode AWS no. E71-T-1C is used. But in WPS E71-T-1 is mentioned. Whether its ok?
  2. PQR in FCAW qualifies 3G position of 27mm plates as per ASME SEc.IX and API-650. What is qualification of position in WPS for 3G whether its ALL POSITION or only 3G postion?
  3. The WPS is to be used for structural activies. ie. as per AWS D1.1. But in WPS also mentioned reference code as ASME sec.IX and AWS D1.1.
Plz clarify.
 
Thanks
 
Arvinda.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...