Re: [MW:11688] Significance of "t" in weldng

In Section IX, t is deposited weld metal thickness
It is given to diffirenciate  in between Base metal thick T and Weld metal t
It is very much usefull in Partial penetration groove and for welder qualification
Pandithan

On Sun, Jul 10, 2011 at 10:42 AM, viral talati <viraltalati.143@gmail.com> wrote:
Dear Devang,
Pls clarify the problem.
but Generally t is used for to show throat thickness.
 
regards

On Sat, Jul 9, 2011 at 11:46 AM, Devang Majithia <dmmajithia@gnfc.in> wrote:
I want to know about the meaning of "t" in weld metal. What does it signifies and what is its importance?
 
Regards,
Devang Majithia
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~ Please don't print this e-mail unless you really need to. Save a tree if possible. ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~  ########################################################################## # Legal Disclaimer :  mail.gnfc.in                                       # # ------------------------------------                                   # # This message may contain confidential and/or privileged information.   # # If you are not the addressee or authorized to receive this for the     # # addressee, you must not use, copy, disclose or take any action based   # # on this message or any information herein. If you have received this   # # message in error, please advise the sender immediately by reply e-mail # # and delete this message.                                               # #                                                                        # # Thank you for your cooperation                                         # ##########################################################################

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...