Monday, July 11, 2011

Re: [MW:11677] LNG Tank Material selection

Dear Limesh,
PNO:-11A,
ASTM A553 Gr 1
Filler Metal Class :-ERiCrFe-9
F NO:43,
A NO;5.11
Thanks
Regards
Uthanmalliah Nagarajan



--- On Mon, 11/7/11, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: [MW:11666] LNG Tank Material selection
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Monday, 11 July, 2011, 2:40 PM

Dear All,


What is the material normally used for LNG(Liquefied Natural Gas) tank fabrication?

I got some information that 9%Ni steel is OK(Still,I am not sure the authenticity of this information).

Apart from 9%Ni,any other material suitable for cryogenic application?

Actually what is this 9%Ni steel?

What is the correct designation of this 9%Ni steel in ASTM?



Regards,

Limesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...