Dear Sir,

 

When project specification and/or your clients requirements demand production test welds than you also have to test the Charpy-V impact properties at required temperatures. This is for verifying that your production achieves the same weld quality as during Procedure Qualification test.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Sanu Krishnan
Verzonden: maandag 11 juli 2011 10:18
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:11664] Poduction impact test

 

Dear experts,

       

  Is it Production imact test required for LTCS,upto -50degree C.Already PQR Test qualified in -50 degree C?

--

SANU.K.NAIR

QC INSPECTOR

DAEWOO E & C

ABUDHABI

Ph: 0507464738

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...