Friday, July 8, 2011

Re: [MW:11637] Impact value in HAZ

Dear Sandeeph..
 

A. As per mr.Dinesh you have to reduce/minimize the heat input as much as low.
B. You can try for any post weld heat treatment..
 
Both will refine your grain size in HAZ so you will get more impact valve.
 
br,
msms
 

 
On Wed, Jul 6, 2011 at 12:29 PM, sandy <sandeepdhiman63@gmail.com> wrote:
Dear All
How we can get better impact values in HAZ with GMAW process in non
alloyed carbon steel?
like with multi pass welding.
Please provide your valuable ideas.

Regards
Sandeep Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...