HI tony..
 
As far as PQR is concerned essential variable is P no only(not Group no) so no need to requalify your procedure with respect to Group no.
 
msms

On Fri, Jul 8, 2011 at 2:16 AM, christopher rajkumar <christopher_rajkumar@yahoo.com> wrote:
Dear Experts...
 
Though my query is basic from ASME SEC IX.....i request you to give me detailed answer and guides from QW 403 AND QW424
 
Question: 1.  PQR qualification with P1 Group 1 to P1 Group 1.....What is the material qualification range??
 
Question:2. PQR qualification with P1 Group 1 to P1 Group 2.....What is the material qualification range??
 
Does PQR qualification with P1 Group 1 to P1 Group 1 qualify even for P1 Group 1 to P1 Group 2.
 
My organisation has previously qualified with ..for example P1G1(SA106 GrB to P1G2 (SA105 Gr 2) with out impact test and in the WPS Qualified material range is given as P1 G1 and P1G2.
 
On what basis this is considered.....please explain.
 
Thank you
 
Tony
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...