Re: [MW:11573] Test required during prouction of API 5L PSL -2 Pipe

Hi all,


   See ISO 3183 CODE.


Regards

2011/7/2 MD AKRAM <mohammedakram2008@gmail.com>
Hi,
For PSL-2 Pipe Mendatory  is all Mechanical Test and X-ray also required.


Ragards,

Sadiq



On Fri, Jul 1, 2011 at 9:24 AM, abhishek ojha <abhishekojha_iu@yahoo.co.in> wrote:
Dear Sir,
Can anyone tell me which are mendatory test required during manfufacturing of PSL-2 pipe.
 
Thanks & Regards,
 
Abhishek Ojha

 Engineer- Construction 

cid:image001.gif@01CA0B94.B49995B0
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...