Monday, May 2, 2011

Re: [MW:10915] any acceptance standards availabe for structural steel? for fitup?

hai friends,
you reffer iscode-7215,structure steel fabrication
tolarence you get all details


best regards
c.saravanan

On 5/2/11, Chandra Bhusan Tripathi <cbt@rediffmail.com> wrote:
> Is it for offshore or onshore?
>
>
> On Sun, 01 May 2011 23:12:58 +0530 wrote
>>Dear all,
>
>
>
> pl tell us..
>
> Any acceptance standards for fitup & fabrication of structural steel..
>
> Like welding codes AWS D1.1, ASME 9.
>
> My client is not specified any codes..
>
> & let me know any codes availabe for fitups like..
>
> Type of joints & how much joints permitable in 6 meter..
>
> type of inserts permitable..
>
> Misalignment permitable..
>
>
>
> Thanks & regards
>
> m
>
>
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
> Chandra Bhusan Tripathi
> 23 Beckett Circle
> Perth, WA
> Australia
> M +61422812970
> H +61862012197
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...