Hi

Please see ASME Sec III NB- 4320 which is about - Welding Qualifications, records and identifying stamps.
Here in NB-4321 (b)(Required qualifications ) it is clearly mentioned that : Procedures, welders and welding operators used to join permanent or temporary attachments to pressure parts and to make permanent or "temporary tack welds" used in such welding shall also meet the qualification requirements of this article and ASME Sec.IX.
In short only qualified welders can be used for Tack welding as per ASME Sec.IX.
Hence qualify your welders on a groove butt joint and use them for tack welding !

Regards

Prem Nautiyal

On Thu, 27 May 2010 20:32:35 +0530 wrote
>You can qualify them with fillet weld test piece, like 1F, 2F etc.



-----Original Message-----

From: Gulam kader

Sent: 27/05/2010 6:03:21 pm

Subject: [MW:5270] Tack welder test



Hi to all,



Please explain how to qualify the welder only for tack weld with code

reference.



Regards,



GKM







--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...