Dear Gulam,
There is no separate qualification for Tack welder.Only qualified welder as per ASME Section IX or as per construction code like AWS D1.1, API 1104 etc.,can do Tack welding.
Regards,
S.Veloumany
From: Gulam kader <armvasi@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, May 27, 2010 3:33:21 PM
Subject: [MW:5270] Tack welder test
Hi to all,
Please explain how to qualify the welder only for tack weld with code reference.
Regards,
GKM
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.