Pl refer para UCS 66, which gives the creteria for governing thickness of varous components in a vessel, including disimilar thick joints, such as nozzle to shell, with ref to figures given elsewhere in this section. If you need more info can provide your joint configuration.

Sent from my Nokia phone
-----Original Message-----
From: Ali Asghari
Sent: 31/05/2010 6:01:26 pm
Subject: [MW:5319] unequal thickness in UCS66

Dear All
according ASME secVIII(DIV1), what is governing thickness in unequal base metals' thickness of a weld joint for impact test?(if tapered or not)
regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...