Re: [MW:5276] Tack welder test

Hi Gulam Kader,
You can go for fillet weld test. You may refer ASME sec.IX, article III  if it is applicable to your project.


With Regards,
Rutvik
Sr.Surveyor
TATA Projects Ltd.

--- On Thu, 27/5/10, Gulam kader <armvasi@gmail.com> wrote:

From: Gulam kader <armvasi@gmail.com>
Subject: [MW:5270] Tack welder test
To: materials-welding@googlegroups.com
Date: Thursday, 27 May, 2010, 6:03 PM

Hi to all,

Please explain how to qualify the welder only for tack weld  with code reference.

Regards,

GKM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...