[MW:5232] Re: Technical Qery regarding welder performance qualification for ASME Sec ix QW-452.1(b)

Dear Mr. Asad Azmi,

Forgot to mention the second part of your questions but QW 452.1(a)
only specifies the tests (specimens) required for welder
qualifications and always QW 452.1 (b) applies for determining the
validity range.

Best Regards,

Herman Pieper

On 23 mei, 07:38, asad azmi <azmiasada...@gmail.com> wrote:
> Dear All,
>
> *Can you please elobrate the meaning of  word "ALL"   and  "1/2 ( 13)  and
> over with a minimum of three layers"  from the table QW - 452.1(b) .*
> **
> *also what is the  thickness of weld metal qualified if the welder is
> qualified by BEND Test.( QW-452.1(a))*
> **
> Thanks & Regards
> **
> *Asad Azmi*
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...