Dear Sandeep,

As electrode manufacturer we recommend maximum 3 years storage under recommended conditions. If you redry them according to the manufacturers recommendation, they will be returned to mint condition. This is sound engineering practice. If the electrodes are packed in an air tight package, they can technically be stored for a very long time. However, there is a limit to how long time documentation is kept by the manufacturer, normally not more than 10 years.

Best regards,


Claes Gillenius




Sandeep Kp <sandeepkp99@yahoo.com>
Sent by: materials-welding@googlegroups.com

2010-05-31 04:20

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
[MW:5300] Expiry date





Dear all,
How many year we can keep E7018 electrode in recomended temperature.
 
With Regards,
 
 
sandeep.k.p

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it.

ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...