Re: [MW:5283] silicon content

There is actually a limit, you have to add the five elements (see ASME Sect II for SA106B) and this should not exceed 1%
 


 
On Thu, May 27, 2010 at 11:46 AM, Sunil <sunilkmani@gmail.com> wrote:
Dear All,

I just want to join two pipes of ASTM A106 Grade B. As per project
speification CE(Carbon Equivalent) permitted as per IIW formula is
0.43   I found that there is no silicon participation in this
formula.But I have come to know that API RP 577 Clause 10.9.1 using a
formula which includes silicon and rest of the part is equivalent to
IIW formula.If we review the standard for ASTM A 106 Grade B for
chemical properties(Table 1 Chemical requirements);we can observe that
the chemical composition has no restriction for silicon (min 0.10 for
all grades) .ie, there is no maximum limit !!! Can we accept
technically an ASTM A 106 Grade B mill certificate with silicon
content ranging from 0.10  to UNLIMITED ??? If not what would be the
maximum acceptable silicon percentage in A106 Grades ?

Thanks and Regards

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...