Re: [MW:5323] Electrode for SA516 Gr.70 Material.

Dear All,
Can we use E7018-G electrode??

Regards,
Vijay



On Mon, May 31, 2010 at 9:06 AM, KOLA Ramalingeswara Rao <krraoind@gmail.com> wrote:
As per ASME Sec II part C, E7018 electrode impact test up to minus 30 degrees C. You can use E7018-1 for  minus 46 degree C.
 
Regards,
 
K.Ramalingeshwara rao.

On Sun, May 30, 2010 at 9:17 PM, Vijay <k.vijayaraj@gmail.com> wrote:
Dear All,

Can we used E7018 electrode for SA516 Gr.70 material (Impact Tested at
-46 oC) or we need to use other??

Kindly clarify.

Regards,
Vijay,
Advanced Oilfield Technology Company,
Oman.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...