You ARE Right Rakesh. It is Lloyds Register Gr A material used for ship building.
arun.
On Mon, May 24, 2010 at 9:36 PM, <rakesh_p1@rediffmail.com> wrote:
I think it should be Lloyd Register A grade material normally used in ship building, if I am not mistaken.
Rakesh PandeyEmpower your Business with BlackBerry® and Mobile Solutions from Etisalat
From: AGUSTIN JIMENEZ <agumarca@yahoo.com>Date: Sun, 23 May 2010 19:12:13 -0700 (PDT)Cc: INSPECTORES DE EQUIPOS ESATICOS<inspectores_equipos_estaticos@gruposyahoo.com>Subject: Re: [MW:5219] LR A GRADE MATERIALHi Manoj.In elbow is large radius (LR) is not grade of material.Best regardsAgustin
De: manoj john <manojacgnr@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: dom, mayo 23, 2010 11:30:22 AM
Asunto: [MW:5218] LR A GRADE MATERIAL
--Dear AllCan anybody give info about LR A grade materialThanks & Regards.Manoj
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments