Re: [MW:5325] silicon content

Mr Soliman is correct, I misread the part on the chemical analysis table


 
On Sun, May 30, 2010 at 8:07 AM, mero soliman <meroman_one@hotmail.com> wrote:
Dear all.

i have checked the SA 106, and i found no limitation in Si%,
but, by experience, in most material test reports i have ever checked, the Si content is (0.2-0.35%) for the carbon steel SA106-B pipes.

- i recommend using the IIW equation in evaluationg the carbon EQUIVALENT, not the API 577 RP Formula, Because the second formula is written as for an example ( i.e : NOT MANDATORY).


Amr Soliman
QA/QC Eng.
petrojet-Egypt



Hotmail: Trusted email with powerful SPAM protection. Sign up now.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...