Dear all.
i have checked the SA 106, and i found no limitation in Si%,
but, by experience, in most material test reports i have ever checked, the Si content is (0.2-0.35%) for the carbon steel SA106-B pipes.
- i recommend using the IIW equation in evaluationg the carbon EQUIVALENT, not the API 577 RP Formula, Because the second formula is written as for an example ( i.e : NOT MANDATORY).
Amr Soliman
QA/QC Eng.
petrojet-Egypt
Hotmail: Trusted email with powerful SPAM protection. Sign up now.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment