Re: [MW:5294] DIN Wire IQI Thickness

Wire IQI
Used to assess sensitivity ; quality of technique 
Pl refer DIN 54109 (1962); ISO 1027
Wire set 1-7; set 6-12; set 10-16 (1,7,6,12,10,16 represent wire numbers)
3 sets - each set having 7 wires (overlapping with adj set) arranged in GP
usually 2% or lesser value of sensitivity is required for general applications
Smaller no 1% indicates higher sensitivity -critical applications

wire dia          wire No
   mm                        
   3.2 ...............  1 
   2.5  ............... 2
   2.0  ............... 3
   1.6   ...............4
   1.25 ...............5
   1.0   ...............6
    0.8  ...............7
---------------------------    
    1.0   ..............6
    0.8  ...............7  
    0.63 ...............8
    0.50................9
    0.40..............10
     0.32..............11
    0.25...............12
-----------------------------
    0.40..............10
    0.32..............11
    0.25..............12
    0.20 .............13
    0.15 .............14  
    0.125............15
    0.10 .............16
  ---------------------------


Regds
MSR
--------------------------------------------------------------------------------------
On Sun, May 30, 2010 at 12:20 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All

Where to we find DIN wire IQI Thickness?
Which standard is deals about DIN wire IQI Thickness?
Where to refer?

--------------------------------------------------------------------------------------------------------------------------------------

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...