Monday, May 24, 2010

[MW:5230] Repaire of Damaged Galvanised Sheet

Dear Friends,

Please advise me whether

1.       we can repair the white rusted GI sheet (Thick 1 – 3.00 mm, ASTM A653, Gr-S340)

2.       or can we re-galvanize the sheet

3.       or for few spots, shall we use some spray but for this A) How to clean  B) its life &  C) visual appearances

 

Best Regards,

M.K.Choudhary

cid:image001.gif@01C5934C.F0F5DF10

P.O. Box 877,  Dammam  31421  KSA

Phone  : (+9663) 8471840 X 555

Fax       : (+9663) 8471291

www.zamilsteel.com

 