Sunday, May 30, 2010

Re: [MW:5302] DIN Wire IQI Thickness

Dear srinivas,
refer ASME section V table 276 for sizes
 

puneet takiar
________________________________

----- Original Message ----
From: Srinivas Engr <srinivas.gmsrini@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Sat, 29 May, 2010 6:50:00 PM
Subject: [MW:5292] DIN Wire IQI Thickness

Dear All

Where to we find DIN wire IQI Thickness?
Which standard is deals about DIN wire IQI Thickness?
Where to refer?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...