Sunday, May 30, 2010

Re: [MW:5296] DIN Wire IQI Thickness

I am not sure, but please try EN 462-1.

With Regads,
Rutvik
Sr.Surveyor
TATA Projects Ltd.

--- On Sun, 30/5/10, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:

> From: Srinivas Engr <srinivas.gmsrini@gmail.com>
> Subject: [MW:5292] DIN Wire IQI Thickness
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Sunday, 30 May, 2010, 12:20 PM
> Dear All
>
> Where to we find DIN wire IQI Thickness?
> Which standard is deals about DIN wire IQI Thickness?
> Where to refer?
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...