  Dear Friend.
 
You should use Plasma Gouging with Hand Torch and use the Flapper disc for cleaning. 
 
 
 
 
 
 

Regards

 

Syed Arshad Farooq 

 QA / QC Engineer

 PROCTER & GAMBLE

 D.L UNIT KARACHI

(+92-21-111-284-284,5378637-40

): +92-308-3067599




From: PB HEGDE <hegde.pb@isgec.com>
To: materials-welding@googlegroups.com
Sent: Wed, March 31, 2010 10:46:01 AM
Subject: [MW:4640] Back gouging of SS

Dear  Friends

 

What is the best method of back gouging of SS weld of heavy thickness plate?

Do you prefer

i)                    Back Gouging by Carbon Arc rod

ii)                   By Plsama gouging with hand torch

 

Ia)If By Carbon Arc rod – How much gouged surface you prefer to grind ? to remove carbon contamination

Iia) Is there any special plasma torch available for back gouging

 

Regards

 

Hegde P.b.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...