Alloy 20 is compatible to deionized water, check the attached guide on Water Deionized row.
I hope you find the proper information.
Regards
JRS
> Date: Thu, 18 Mar 2010 12:29:12 +0530
> Subject: [MW:4578] Alloy 20 in DI Water service
> From: e1500603@gmail.com
> To: materials-welding@googlegroups.com
>
> Hi
>
> can Alloy 20 (3-4% Cu) be used in De Ionised Water ??
> anbody used this combination ?
>
> Thanks
>
> Satish.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hotmail has tools for the New Busy. Search, chat and e-mail from your inbox. Learn More.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment