In my opinion low carbon content of SS304L will help in avoiding carbide precipitation.
 
best regards.
 
Sunil Mathur

On Sat, Nov 28, 2009 at 7:47 PM, sachin sankhe <sachin.sankhe@rediffmail.com> wrote:
Dear Freinds,
I have query on below subject

We have got main colum section of FCC unit wherein base metal is LAS cladded with SS304L.This requirement in specified by UOP Process Licensor
However design temp of Main column is around 55o deg.C
Under this circumstances,I feel SS304L is not suitable at this temp since it will result in formation of chromium carbide at grain boundries.
I feel UOP shall have specifed SS347.
Kindly share your knowledeg

Regards
Sachin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...