Dear All

 

As per the SA 516 GR 70, boron content is not specified and shall not be present as specified element. For SA 516 GR 70 plate  manufacturer certifies that this element is within permissible limit

 

Kindly give your suggestions to what basis we can certify for Coded vessels being constructed

 

Also kindly brief as to why the presence of boron and its affect??

 

 

Thanks in advance & regards

 

Prashanth Hegde

Head Quality

 



Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...