Prashanth,

 

Well bristles soluble salt test can be carried out. All you need is the standard bristles  kit with digital meter, patches, syringe etc. provided in the kit.

 

Regards

Rajneesh

 

From: Qamlr [mailto:qamlr@cicb-chemicon.com]
Sent: Wednesday, November 25, 2009 12:05 PM
To: materials-welding@googlegroups.com
Subject: [MW:3738] FW: CICB Painting facility and process qualification approval

 

Dear All

 

Request your suggestions as to how we can carry out the salt contamination test on job before blasting.. If the salt is > 7 micro gram/cm, then we have to clean the entire surface with water jet .This is recommeded by our client as our manufacturing facility is close to coast.

 

 Thanks & regards

 

Prashanth Hegde

Head Quality

CICB-Chemicon Pvt. Ltd

Mangalore- INDIA

 

 


Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...