Dear Mr. Hegde,
To do the salt test on the blasted surface and prior to blasting kit is available in market.(Bressel's kit)
There is a patch type thing which you paste on the surface. Then inject distiled water in it. Rub the patch water on the substrate. So the salt contain on the surface dissolved in water. And again suckout this water by injection. And test the salt contain with the digital instrument included in the KIT.

Best Regards,

Nilesh Pathare
NDT Level III, CSWIP BGAS painting gr.2,
Sharptest NDE & Inspection services, Mumbai.
On Wed, Nov 25, 2009 at 12:04 PM, Qamlr <qamlr@cicb-chemicon.com> wrote:

Dear All

 

Request your suggestions as to how we can carry out the salt contamination test on job before blasting.. If the salt is > 7 micro gram/cm, then we have to clean the entire surface with water jet .This is recommeded by our client as our manufacturing facility is close to coast.

 

 Thanks & regards

 

Prashanth Hegde

Head Quality

CICB-Chemicon Pvt. Ltd

Mangalore- INDIA

 



Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...