RE: [MW:3736] Bolts/Nuts Material

As ASTM A193 bolts are not stainless steel there is no issue with oxide film

 

Best regards,

 

John Lock

Quality & Classification Engineer

Pacific Deepwater Construction Ltd

cid:image002.jpg@01CA4F2E.75D71400

Cellular.                 +82 (0)10 4693 6282

Office Tel.              +82 (0)55 631 9071

Office Fax.             +82 (0) 631 7499

E-mail                    j.lock@pacificdrilling.com

P Before printing I think about the environment

 

From: Ohm-Srinivasulu. K [mailto:nirgunaya@yahoo.com]
Sent: Wednesday, November 25, 2009 3:12 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:3735] Bolts/Nuts Material

 

RP,

 

Thanks, I should not deviate from company specs, what I can do is whether to approve the vendor proposal or not.

on A193 GR. B8 HDG may not stick unless zinc penetrates the passive oxide film on SS

Does A193 Gr. B7 material can be HDG?


ohm guru namasivaya

--- On Wed, 11/25/09, Ramprasad Chari <ramprasad.chari@gmail.com> wrote:


From: Ramprasad Chari <ramprasad.chari@gmail.com>
Subject: Re: [MW:3732] Bolts/Nuts Material
To: materials-welding@googlegroups.com
Date: Wednesday, November 25, 2009, 9:26 AM

Zinc Electroplating is not a very durable/useful coating.Its thk is also around 15 microns only.Better ones are Cadmium Plating,Hot Dip galvanizing and Barium carbonate coating.

Regards

Aarpee

On Tue, Nov 24, 2009 at 6:30 PM, Ohm-Srinivasulu. K <nirgunaya@yahoo.com> wrote:

HI,

 

I want to clarify a deviation request from Valve vendor,

As per the client specs,

 

For Bolting for Bonnet, Packing-box etc

All carbon steel or low alloy steel bolting shall be zinc plated(elctro-deposited), bichromated.

 

but vendor is proposing

 

Our proposal for A216 WCC Body (Non-Sour) as follows;

Body Studs & Nuts (21000 Series): A193 Gr.B7 / A194 Gr.2H zincplated

(without chromated)

Body Studs & Nuts (35002 Series): A193 Gr.B8 CL.1 / A194 Gr.8

Gland Studs & Nuts : A193 Gr.B8 CL.1 / A194 Gr.8

 

so my dout is in humid areas like Japan we need the bolts to be

Zincplated/bichromated to prevent white rust and in hot areas like

Qatar its not required. 

Please confirm my understanding,

(As the specs were basically developed by JGC they specified as

zinc plated/bichromated)

 

 

Ohm-Srinivas

Sr. Piping Engg.

ohm guru namasivaya

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...