Dear Anant,

5% fibre elongation is the limit for Carbon and low alloy steel. For stainless steel it is 15-20%. We have to refere UHA-44 and table UHA-44 where the requirement are clearly mentioned.

Hope this will help to make decision.

Regards.
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector
 

2009/11/17 ANANT ONKAR <jointcross@hotmail.com>
Dear Pl. check what percentage elongation is coming while cold forming if it is more than 5 % you have to do heat treatment.
Regards
Anant 
 

From: AshokKumar@Zamilsteel.comDate: Mon, 16 Nov 2009 11:01:04 +0300
Subject: [MW:3666] Re: Cold form dish


Dear Devang Patel

 

                If u r doing cold forming no heat treatment is required for both CS & SS material

Regards

P.Asok Kumar

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: Monday, November 16, 2009 9:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:3664] Cold form dish

 

Can any one know about SA-240 type 304LN or X2CrNiN 18-10(1.4311)material?

If we make cold form dish than heat treatment is required or not??

 

 

Regards,
Devang Patel | Manager Engineering
Inox India Ltd. | 4th Floor, ABS Tower, Old Padra Road, Vadodara. Guj. India.
Voice: + 91-265-3056100 ext. 392 | Fax: +91-265-2341449 | Mobile: +91 9879803401
Email: devangp@inoxindia.com | web: www.inoxindia.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

2 comments:

Anonymous said...

It is very interesting for me to read that article. Thank author for it. I like such themes and anything connected to them. I would like to read more on that blog soon.

Anonymous said...

Pretty interesting blog you've got here. Thanx for it. I like such topics and anything that is connected to this matter. BTW, try to add some photos :).

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...