Thursday, November 26, 2009

Re: [MW:3752] Welding of SA 537

E7018-1 with low hydrogen can do the job


Dr. G. Dilintas
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118