Thursday, November 26, 2009

[MW:3750] Welding of SA 537

Can anyone tell me to weld the below material with SMAW which
electrodes we have to use , to weld with SAW which filler wire & flux
combination we have to use.
The material and test requirement is as below…

 Material is SA-537 Class 1, Fully Killed, Normalized, Charpy V-
Impact Tested
 Material is SA-516 Gr.70, Fully Killed, Normalized
 Thickness varies from 38 mm to 50 mm for both materials.
After complication of welding we have to test PTC (production test
coupon) @ -48˚C (Negative 48). The impact energy value shell be 50
joule.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...