Wednesday, November 18, 2009

Re: [MW:3686] RE: 3678] POSITIONS IN overlaying

the position is  4G in case of overhead welding.

WITH WARM REGARDS 
  ANKIT GUPTA 
    
Er@BHEL

--- On Wed, 11/18/09, PB HEGDE <hegde.pb@isgec.com> wrote:

From: PB HEGDE <hegde.pb@isgec.com>
Subject: [MW:3682] RE: 3678] POSITIONS IN overlaying
To: materials-welding@googlegroups.com
Date: Wednesday, November 18, 2009, 9:22 AM

In 3 G will qualify for all position

 

Hegde

 

From: Ali Asghari [mailto:asghariali@rocketmail.com]
Sent: Tuesday, November 17, 2009 6:17 PM
To: materials-welding@googlegroups.com
Subject: [MW:3678] POSITIONS IN overlaying

 

Hi All

are overlaying positions same with groove positions?(according ASME IX)

best regards.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...