Re: [MW:3721] P No- 1 Material

I am giving my opinion based on experience.

As HIC requirements are there PWHT has to be carried out at minimum 620 C to maintain the hardness within limit. On the other hand thickness of Plate is 132mm where after simulation of 11 hrs Tensile properties goes down specially in core (middle crosssection of plate). When tensile test from 1/4 T or 1/2 T taken there are possibility that UTS value goes below 485MPa.

Solutions

1)If client spec does not specify for simulation of extra cycle, ask mill to do test for reference and if pass no issues. If it fails just keep those value for reference.

2)Try to convinve Client to accept the PWHT Cycle with lower soaking time (ASME). I am not sure which design / manufacturing code is being used.

3)Check with design people if you use Gr 60 or Gr 65 instead of Gr 70, so that dropping of tensile strength can be taken care. These grades Mills can supply easily

Regards.
CK

   

2009/11/23 Rana, Jignesh <jignesh.r@thyssenkrupp.com>
 
Dear All,
 
I have an equipment to be installed in sour services.
 
Material – SA 516 Gr. 70 (HIC tested plates), 132 mm thickness.
 
For PWHT the soaking time is 5.30 Hrs as per project specification. Considering one cycle for future site / modification requirement, the total simulation time works out to be 11 Hrs.
 
PWHT Temperature – 620 Deg .C.
 
What would be behavior of material below LOWER TRANSFORMATION TEMPERATURE (P No. 1), against this cycle? (Tensile property, Impact property).
 
All reputed mills are denying for supply with the simulated testing condition (620 DEG C and 11 Hrs. Soaking Time).
 
Regards,
 
JIGNESH R RANA
 

Messages sent by email can be manipulated by third parties and are therefore generally not legally binding. This message contains confidential information that may be privileged or protected from disclosure. If you are not the intended recipient, please be advised that you have received this email by mistake. You are requested to notify us immediately by return email and delete this email from your system. Any use, copying, distribution or printing of information by the unintended recipient is strictly prohibited. Thank you.

Regd. Office: Uhde House, Vikhroli (West), Mumbai 400 083, India
Tel: 91-022-6796 8000, Fax: 91-022-2578 4327 Website: www.uhdeindia.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...