Dear All,
 
I have an equipment to be installed in sour services.
 
Material – SA 516 Gr. 70 (HIC tested plates), 132 mm thickness.
 
For PWHT the soaking time is 5.30 Hrs as per project specification. Considering one cycle for future site / modification requirement, the total simulation time works out to be 11 Hrs.
 
PWHT Temperature – 620 Deg .C.
 
What would be behavior of material below LOWER TRANSFORMATION TEMPERATURE (P No. 1), against this cycle? (Tensile property, Impact property).
 
All reputed mills are denying for supply with the simulated testing condition (620 DEG C and 11 Hrs. Soaking Time).
 
Regards,
 
JIGNESH R RANA
 

Messages sent by email can be manipulated by third parties and are therefore generally not legally binding. This message contains confidential information that may be privileged or protected from disclosure. If you are not the intended recipient, please be advised that you have received this email by mistake. You are requested to notify us immediately by return email and delete this email from your system. Any use, copying, distribution or printing of information by the unintended recipient is strictly prohibited. Thank you.

Regd. Office: Uhde House, Vikhroli (West), Mumbai 400 083, India
Tel: 91-022-6796 8000, Fax: 91-022-2578 4327 Website: www.uhdeindia.com

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...