[MW:3677] Re: welder base matel qualification

Dear Mr.Raghavan

Essential variables for Welder qualification are given in QW350 of
ASME IX. Looking to the tables for seperate welding processes you can
see they always refer to QW403.18 for P. no's qualified. First of all
material need to be listed in QW 422, if so look to the materials P.
no. and now look at QW 423 if this material is in the range of the
table under QW 423.1. When having a welder qualified for P. no. 1 you
can see in this paragraph that he is qualified for P. no. 1 throug P.
no. 11, P. no. 34 and P. no. 41 through P. no. 49.

Best regards,

Herman Pieper

On 16 nov, 12:23, babu raghavan <babuprm...@yahoo.com> wrote:
>  
> dear all
>  
> As per sec ix,
> welder test performing p1 to p1 ,test cuopon. what is the welder  range of qualification in base matel.
>  
>  
> babu. 
>
>  
>  
>
>       The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.http://in.yahoo.com/

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...