[MW:3674] Re: welder base matel qualification

Refer QW-423.1

Regards,

On 11/16/09, babu raghavan <babuprmech@yahoo.com> wrote:
>
> dear all
>
> As per sec ix,
> welder test performing p1 to p1 ,test cuopon. what is the welder  range of
> qualification in base matel.
>
>
> babu.
>
>
>
>
>
>
> The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.
> http://in.yahoo.com/
> >
>


--
Sukamal

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...