Is it mandatory to demonstrate NDT procedure qualification before applying in the actual job? If so, please give the code/standard reference.
 
Regards
Hrishi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

2 comments:

Anonymous said...

I don't think so Hrishi. Most specs lay out guidelines of what you need to achieve or prove. You should provide a technique sheet, which outlines exactly how you plan on doing the job, ( if its an xray job, you should include equipment, Kv, Ma, distance, film screens, exposure time etc...with exact values for each), but it is very specific to the job in question and if you use different techniques you should have different technique sheets for each.

Sometimes it is impossible to predict exactly how things will work out, so you basically have to suck it and see at times

Chris said...

According to ASME Code: Section V - Nondestructive Examination, "A procedure demonstration shall be performed to the satisfaction of the Inspector" (Par. T-150(a), 2007Ed/2008Addenda). Typically not necessary for typical procedures unless special procedures are used. But, it is up to the Inspector if the procedure is satisfactory in their opinion.

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...