Re: [MW:3754] Re: Pickling and Passivation


Flushing with abundant DM water is essential for cleaning after pickling and passivation.The presence of acid stains can be tested with litmus paper.
regards
M.S.R.K.Srinivasa Prasad
Sr. Manager( Mech. Maint  PP-1)
Nagarjuna Fertilizers And Chemicals
Nagarjuna Road
KAKINADA-533003
Ph: 0884-2360212(O)
                 2379302(R)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...