[MW:3693] Re: Tolerance for Pitting of plates

There is no code available for pittings acceptance; any raw material
shall be free from surface defects; so the pittings coming under
surface defects. The acceptance to the pitting on the surface is
depending upon the usage which should not disturb the minimum design
thickness.


On Nov 18, 1:00 pm, Mrityunjay Kumar / ZS Saudi PEB QA/QC
<Mrityunjayku...@zamilsteel.com> wrote:
> Dear all,
> Can any body guide or send me the tolerance for pitting of plates (ASTM A572M Gr-50)?
> Quick reply will be highly appreciated.
>
>  Thanks and Regards,
> M.K.Choudhary
>       [cid:image001....@01CA683E.59299980]
>       PEB - QA/QC
> P.O. Box 877, Dammam 31421
> Kingdom of Saudi Arabia
> '   +966 38471840 Ext- 555
> 7    +966 38471840 Ext-559
> ý  www.zamilsteel.com<http://www.zamilsteel.com>
>
> ---------------------------------------------------------------------------­-----------------------------
> Disclaimer: This email and any files transmitted with it are confidential
> and intended solely for the use of the addressee(s) named herein. If you
> are not the intended recipient or addressee, you should not use, disseminate,
> distribute, copy or alter this email. Any views or opinions presented in this
> email are solely those of the author and might not represent those of "Zamil
> Industrial" and or its units.
>
> Warning: Although reasonable precautions have been taken to ensure no viruses
> are present in this email, the company cannot accept responsibility for any
> loss or damage arising from the use of this email or attachments. If you have
> received this electronic mail message in error, please contact the sender directly.
>
>  image001.png
> 2KViewDownload

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...