Tuesday, November 17, 2009

RE: [MW:3679] Re: Cold form dish

Dear Pl. check what percentage elongation is coming while cold forming if it is more than 5 % you have to do heat treatment.
Regards
Anant 
 

From: AshokKumar@Zamilsteel.com
To: materials-welding@googlegroups.com
Date: Mon, 16 Nov 2009 11:01:04 +0300
Subject: [MW:3666] Re: Cold form dish

Dear Devang Patel

 

                If u r doing cold forming no heat treatment is required for both CS & SS material

Regards

P.Asok Kumar

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: Monday, November 16, 2009 9:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:3664] Cold form dish

 

Can any one know about SA-240 type 304LN or X2CrNiN 18-10(1.4311)material?

If we make cold form dish than heat treatment is required or not??

 

 

Regards,
Devang Patel | Manager Engineering
Inox India Ltd. | 4th Floor, ABS Tower, Old Padra Road, Vadodara. Guj. India.
Voice: + 91-265-3056100 ext. 392 | Fax: +91-265-2341449 | Mobile: +91 9879803401
Email: devangp@inoxindia.com | web: www.inoxindia.com


 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
--------------------------------------------------------------------------------------------------------
Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use, disseminate,
distribute, copy or alter this email. Any views or opinions presented in this
email are solely those of the author and might not represent those of "Zamil
Industrial" and or its units.

Warning: Although reasonable precautions have been taken to ensure no viruses
are present in this email, the company cannot accept responsibility for any
loss or damage arising from the use of this email or attachments. If you have
received this electronic mail message in error, please contact the sender directly.



New Windows 7: Simplify what you do everyday. Find the right PC for you.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...