Monday, November 16, 2009

[MW:3675] Re: Welder qualification

According ASME IX, QW-432 and QW-433, if the welder was qualificated both with backing or witouth backing, with F-N°2 (E-6013), he can´t weld material Filler F-N°3 (E-6010).
About API 1104, the E-6013  is not include on the grouping to filler material.
Regards Ruscitto
 
>>> Santhosh V S <santhosh.1974@yahoo.com> 16/11/2009 08:52:00 am >>>
Dear All,
 
We have one WPS with E6010 root and E6013 sebsequent passes.We have to qualify some welders using E6013 electrode for both root and other passes. Can anybody advise me that whether we can use the above WPS for that welder qualification?
 
Regards
 
Santhosh


*********************************************************************

¡IMPORTANTE!

Para evitar accidentes por inhalación de monóxido de carbono:

- Mantenga los ambientes ventilados en forma permanente.

- Revise que la llama sea color azul y uniforme.

- Instale y haga revisar periódicamente sus artefactos sólo a través de gasistas matriculados.

Recuerde que los artefactos a gas pueden emitir Monóxido de Carbono: un gas altamente tóxico e imperceptible.

Más consejos en http://www.metrogas.com.ar

*********************************************************************

Este mensaje es privado y confidencial y va dirigido sólo al destinatario indicado. Si lo ha recibido por error, por favor avísenos inmediatamente vía e-mail a error-mail@metrogas.com.ar y tenga la amabilidad de eliminarlo de su sistema. La utilización o divulgación de su contenido puede importar la comisión de un delito. No copie, reproduzca o divulgue -en forma parcial o total- su contenido. Cualquier opinión contenida, es exclusiva de su autor y no representa la opinión de MetroGAS S.A. - Muchas gracias.

This message is private and confidential and it is only intended for the addressee named above. If you have received this message and it is not addressed to you, please advise us immediately at error-mail@metrogas.com.ar and kindly remove it from your system. The use or disclosure of its contents may be regarded as an offense. Do not copy, reproduce or disclose them, either partially or fully. Opinions are the exclusive responsibility of the author and do not represent the opinion of MetroGAS S.A. - Thank you.

:: http://www.metrogas.com.ar

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...