Dear Santhosh
 
First of all you must specify the relevant code and standard. For example based on AWS D1.1, if the classification of electrodes were same, you could implement the qualified welders of each one for the other.
 
Yours truly,
Keyvan

 
On 11/16/09, Santhosh V S <santhosh.1974@yahoo.com> wrote:
Dear All,
 
We have one WPS with E6010 root and E6013 sebsequent passes.We have to qualify some welders using E6013 electrode for both root and other passes. Can anybody advise me that whether we can use the above WPS for that welder qualification?
 
Regards
 
Santhosh
 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...