Dear all,
You should make the paint on test block with the same condition in test object and do transfer correction same as procedure with Bhaskar kale.
Best regards,
TRAN VAN VUONG
Email: vuongtv@phateco.com
From:
Sent: Monday, November 16, 2009 5:17 PM
To:
Subject: [MW:3669] Re: ultrasonic testing
Dear Mr Bhaskar kale
thank you for responding.
but the calculation of transfer correction is permitted for this case(existed thickness paint )or not?if yes in wich standard or technical document?
regard adv.
From: "Kale, Bhaskar M" <bmkale@gmail.com>
To:
Sent: Mon, November 16, 2009 12:57:52 PM
Subject: [MW:3668] Re: ultrasonic testing
Hello Mr. Ali Asghari ,
Do the transfer correction as per the attached procedure.
This will compensate for the thickness of the paint.By adding the transfer correction sensitivity in the test material will remain same.
If you have any problem in the present job…just refer to the code of construction and cross reference by code of construction if any.
Regards, Bhaskar kale
On Mon, Nov 16, 2009 at 3:34 PM, Ali Asghari <asghariali@rocketmail.com> wrote:
hi friends
in any standard or code, is specified the permitted maximum thickness of paint that don't interfer with Ultrasonic testing?
best regards
--
Regards,
Bhaskar Kale
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments