Wednesday, June 17, 2009

[MW:2461] Re: EEMUA 144.1 Standard availability

if it is CuNi offshore applications try with http://www.sitindustriemarine.com/.
they have 14barg range, but i think its as per BS or EN stds, you may
convinec your client
i don't know still this publication is valid as this requiremnt i have
seen in even ONGC stnadrads a decade back.

check these links

http://www.marine-applications.com/offshore-products/pipes/seamless-pipes/of-pr_pi_se-pi_index.php.en
http://www.athical.com/pdf/Page%20011.pdf
http://www.nautic.co.uk/pipes.html


On Jun 17, 9:26 am, BR <raghurambath...@gmail.com> wrote:
> for what material grade?
> is it 14 barg or 16 barg will do instead?
>
> On Jun 17, 9:10 am, ptvvtp <cezon...@gmail.com> wrote:
>
>
>
> > We are facing a problem wherein we do not have the pipe thicknesses
> > for a 14 barg system. Our client's bid document specifies EEMUA 144.1
> > for a 14 barg system. I would like to know the availability of the
> > same in the market and the corresponding thicknesses of the same.- Hide quoted text -
>
> - Show quoted text -
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...